by Won-hui Lee |
1/700 IJN Musashi - Sibuyan Sea (Fujimi)
I made a mistake. The resin hardener ratio was too high. So, Musashi was melted by high heating temperature.
My initial intention was to lean toward the left side 5 degrees. But contrary to my intention, as the resin shrank, it leans almost 30 degree. Therefore, I was forced to ignore the historical investigation.